Optimum Brazing Conditions for Joining Commercially Pure Titanium to 304L Stainless Steel using BAg-8 Silver Filler Metal

Document Type : Original Articles

Authors

Materials engineering faculty, Islamic Azad University of Najafabad, Iran

Abstract

Joining of titanium alloys to other materials especially steels has attracted much attention in recent years due to the exceptional properties of titanium such as excellent corrosion resistance and mechanical properties and its increasing application in various industries. According to the Fe-Ti binary phase diagram, these two elements do not have complete solubility. This leads to difficulties during fusion welding of these two alloy. One of the best methods for joining dissimilar alloys is brazing. In this research, the metallurgical and mechanical properties of brazing lap joints of steel to commercially pure titanium using a commercial filler metal (BAg-8) made under different time and temperature conditions were investigated. The study of the microstructure interface shows the formation of a chemical layer close to the titanium side of the joint, while no chemical compounds were created on the steel side. A coarse structure is formed at the interface between the steel and silver solder alloy. The observed coarse grain structure is related to the grain growth along with recrystallization in the steel substrate at high temperatures. Analysis of the joints was carried out by optical microscopy, scanning electron microscopy, X-ray diffraction and hardness measurements. The results show that with increasing temperature, as well as brazing time, the average shear strength decreases due to the increased thickness of the intermediate layer.

Keywords


1. He P., Feng J.C., Xu W., "Interfacial microstructure of induction brazed joints of TiAl-based intermetallics to steel 35CrMo with AgCuNiLi filler", Materials Science and Engineering A, Vol. 408, pp. 195–201, (2005).
2. Ghosh M., Chatterjee S., Mishra B., "The effect of intermetallics on the strength properties of diffusion bonds formed between Ti–5.5Al–2.4V and 304 stainless steel", Materials Science and Engineering A, Vol. 363, pp. 268–274, (2003).
3. Chan H.Y., Liaw D.W., Shiue R.K., "The microstructural observation of brazing Ti–6Al–4V and TZM using the BAg-8 braze alloy", International Journal of Refractory Metals & Hard Materials, Vol. 22, pp. 27–33, (2004).
4. Elrefaey A., Tillmann W., "Microstructure and mechanical properties of brazed titanium/steel joints", Journal of Material Science, Vol. 42, pp. 9553–9558, (2007).
5. Lee W.B., Lee C.Y., Chang W.S., Mo Yeon Y.," Microstructural investigation of friction stir welded pure titanium", Materials Letters, Vol. 59, pp. 3315-3318, (2005).
6. Laik A., Shirzadi A.A., Tewari R., Kumar A., Jayakumar T., Dey G.K., "Microstructure and Interfacial Reactions During Active Metal Brazing of Stainless Steel to Titanium", The Minerals, Metals & Materials Society and ASM International, (2013).
7. Yue X., He P., Feng J.C., Zhang J.H., Zhu F.Q., "Microstructure and interfacial reactions of vacuum brazing titanium alloy to stainless steel using an AgCuTi filler metal", Journal of Materials Characterization, pp. 1721–1727, (2008).
8. Elrefaey A., Tillmann W., "Brazing of titanium to steel with different filler metals: analysis and comparison", Journal of Materials Science, pp. 4332-4338, (2010).
9. Petzow G., Effenberg G., "Comprehensive compendium of evaluated constitutional data and phase diagrams", Weinheim, Germany, pp. 14-17, (1998).
10. Phillips V.A., "A metallographic study of precipitation in a Ni-12.7 at.% Al alloy" Acta Metallurgica, Vol. 14, No. 11, pp. 1533-1547, (1966).
11. Elrefaey A., Tillmann W., "Brazing temperature determines the microstructure and mechanical behavior of steel/titanium brazed joints", IBSC, Orlando, FL, pp. 2-5, (2009).
12. Baker H., "ASM handbook alloy phase diagrams", ASM International, Materials Park, OH, pp. 119-123, (1992).
13. Shiue R.K., Wu S.K., Li I.H.,"Infrared brazing of Fe3Al intermetallic compound using gold-based braze alloy", Gold Bull, pp. 49-56, (2011).
14. He P., Feng J.C., Xu W., "Microstructure and kinetics of induction brazing TiAl-based intermetallics to steel 35CrMo using AgCuTi filler metal", Materials Science and Engineering A, Vol. 418, pp. 53-60, (2006).
15. Murakami T., Nakata K., Tong H., Ushio M.,"Dissimilar Metal Joining of Aluminum to Steel by MIG Arc Brazing Using Flux Cored Wire", ISIJ International, Vol. 43, No. 10, pp. 1596-1602, (2003).
16. Shiue R.K., Wu S.K., Shiue J.Y., "Infrared brazing of Ti–6Al–4V and 17-4 PH stainless steel with (Ni)/Cr barrier layer(s) ", Materials Science & Engineering A, Vol. 488, No. 1, pp. 186-194, (2008).
17. Shin C.K., Huh J.Y.," Effect of Cu-containing Solders on the Critical IMC Thickness for the Shear Strength of BGA Solder Joints", Third proceeding of EPTC, pp. 406–411, (2000).
CAPTCHA Image